Abstract

FERRO-TIC HT-2 is a dispersion of extremely hard titanium carbide grains in an austenitic, heat-resistant, age-hardenable, iron-nickel-chromium alloy matrix. It exhibits good strength and good resistance to oxidation, corrosion, carburization and wear up to 1350 F. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as creep. It also includes information on corrosion resistance as well as heat treating, machining, joining, surface treatment, and powder metal forms. Filing Code: SS-322. Producer or source: Chromalloy American Corporation, Sintercast Division.