Abstract

CRUTEMP 25 is a fully austenitic stainless steel with outstanding resistance to scaling at elevated temperatures. It also has high strength at elevated temperatures and its weldability is excellent. It is used in such applications as automotive emission control systems and gas turbines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-309. Producer or source: Crucible Stainless Steel Division, Colt Industries.