PYROMET 350 is a chromium-nickel-molybdenum stainless steel that can be hardened by transformation to martensite and/or preciptation hardening. It is used for gas turbine components and similar parts where high strength is required at room intermediate temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-296. Producer or source: Carpenter Technology Corporation.