Abstract

ALLEGHENY STAINLESS TYPE 434 is a low-carbon ferritic stainless steel with good corrosion resistance to mildly corrosive environments and the atmosphere. It is oxidation resistant at temperatures up to 1600 F for intermittent service and up to 1450-1500 F for continuous service. It is used for automotive trim and other exterior environments. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-292. Producer or source: Allegheny Ludlum Corporation.