ALLEGHENY TYPE 332 is an austenitic stainless steel developed to resist oxidation and carburization at elevated temperatures. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-279. Producer or source: Allegheny Ludlum Corporation.