CA-6NM is a cast stainless steel that has good resistance to cracking during and after solidification of heavy sections, and good weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-269. Producer or source: Alloy steel foundries.