Abstract

Joslyn Stainless Type-305H is a modified austenitic chromium-nickel steel recommended for severe cold heading applications because of its low work-hardening factor. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-178. Producer or source: Joslyn Stainless Steels.