Abstract
SANDVIK SANICRO 31 is an iron-nickel-chromium alloy having good resistance to corrosion and oxidation and good mechanical properties at elevated temperatures. It is recommended for electrical sheathing, pyrometer tubes, equipment for heat treating and furnace tubes and other equipment in the petrochemical industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-172. Producer or source: Sandvik.
chemical composition, corrosion-resistant alloys, elasticity, electrical sheathing, furnace tubes, hardness, heat treatability, high-temperature alloys, joinability, machinability, oxidation resistance, petrochemical equipments, physical properties, pyrometer tubes, SANDVIK SANICRO 31, tensile properties, workability
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Stainless steel
Corrosion-resistant alloys
High-temperature alloys
Furnace tubes
Chemical composition
Oxidation resistance
Heat treatability
Joinability
Machinability
Workability
Elastic modulus
Hardness
Tensile properties
Physical properties
Thermal properties
Chemical and petrochemical processing equipment
Electrical systems
You do not currently have access to this content.