CALITE B-29 is a high chromium-nickel heat resistant casting alloy having excellent oxidation and carburization resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-76. Producer or source: Calorizing Company.