Abstract
FAHRALLOY 2817 is a 28% Cr-16% Ni heat and corrosion resistant casting alloy. It is non-hardenable and corresponds to A.C.I. Type HI alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-74. Producer or source: Fabralloy Canada Ltd.