ARMCO 17-14 Cu-Mo is an austenitic stainless steel which responds favorably to an age-hardening heat treatment. It is recommended for highly stressed stainless steel parts requiring long service at temperatures up to 1500 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-68. Producer or source: Armco Inc., Eastern Steel Division.