Abstract

TENELON is a chromium-manganese-nitrogen grade of austenitic stainless steel with high tensile strength and ductility in the annealed condition as well as very attractive elevated temperature properties. This datasheet provides information on composition, hardness, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-60. Producer or source: United States Steel Corporation.