Abstract

UNILOY 19-9DL is a chromium-nickel heat resistant super alloy, capable of withstanding high static and dynamic stresses through at least 1200 deg. F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-19. Producer or source: Cyclops Corporation.