Strenx 900 Plus is a structural steel with a minimum yield strength of 900 MPa (131 ksi). Strenx 900 Plus provides a good combination of strength and toughness together with good workshop properties. Typical applications include load-bearing structures, where low weight is needed. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-826. Producer or source: SSAB Swedish Steel Inc..