FERRO-TITANIT C-SPEZIAL is one of a series of metal-matrix composites manufactured by a powder metallurgy process. Ferro-Titanit C-SPEZIAL contains 33% titanium carbide, one of the hardest and most resistant carbides. Because of its high wear resistance and low tendency towards cold welding, Ferro-Titanit is particularly used in forming and cutting tools. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and compressive and bend strength. It also includes information on wear resistance as well as forming, heat treating, machining, and powder metal forms. Filing Code: SA-812. Producer or source: Deutsche Edelstahlwerke GmbH.