Abstract

Ympress Laser E250C (EN 10025-2) is a hot-rolled structural steel. It is optimized for efficient laser cutting and post-cut processing. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming. Filing Code: SA-747. Producer or source: Tata Steel.