Abstract

SPARTAN II (HSLA-100) is one of the family of Spartan high strength (>690 MPa, or >100 ksi, minimum yield strength), high toughness, improved weldability steels, which are alternatives to traditional quenched and tempered alloy steels. The Spartan family of steels are low carbon, copper precipitation hardened steels. Spartan II has improved yield strength compared to Spartan I. This datasheet provides information on composition, physical properties, microstructure, tensile properties. It also includes information on forming and joining. Filing Code: SA-738. Producer or source: ArcelorMittal USA.