DI-MC 460 is a weldable fine-grained thermomechanically rolled steel for structural design. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-717. Producer or source: Dillinger Hütte GTS.