CBS-223 VIM-VAR is a double vacuum-melted carburizing bearing and gear steel. This datasheet provides information on composition, physical properties, microstructure, and elasticity. It also includes information on forming and heat treating. Filing Code: SA-716. Producer or source: Latrobe Specialty Steel Company.