Abstract

Cryelso 3.5 is a steel alloy designed for low temperature applications and requiring high impact values. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on low temperature performance as well as forming, heat treating, and joining. Filing Code: SA-670. Producer or source: Industeel USA, LLC.