Abstract

Abrazo 400 is roller quenched to obtain high strength, good properties, and excellent wear resistance. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear and bend strength It also includes information on wear resistance as well as forming, machining, and joining. Filing Code: SA-648. Producer or source: Corus Long Products.