Abstract

CarElso 60/65 is a steel alloy with special melt practice producing a pressure vessel material with resistance to mild sour service. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-635. Producer or source: Industeel USA, LLC.