Abstract

Ovako 146S is an ingot cast case-hardening steel with good dimensional stability and high toughness. This datasheet provides information on composition as well as fatigue. It also includes information on casting, heat treating, and machining. Filing Code: SA-601. Producer or source: Ovako North America Inc. and Ovako Holdings AB.