OvaX 800 is a through-hardening steel for bearing and transmission applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on casting, forming, and machining. Filing Code: SA-596. Producer or source: Ovako North America Inc.