Abstract

Ferrium C61 is a case/core alloy with ultrahigh strength and excellent fracture toughness. It is used in gears and a number of automotive racing applications. This datasheet provides information on tensile properties. It also includes information on forming and heat treating. Filing Code: SA-551. Producer or source: QuesTek Innovations, LLC.