Docol 100DP is a very-high-strength steel that is used for transportation and structural products. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on joining. Filing Code: SA-519. Producer or source: SSAB Swedish Steel Inc.