Abstract

V and M T/P92 is a ferritic alloy with improved high-temperature strength and creep behaviors compared to those of other ferritic steel alloys. Applications include both superheater tubes and main steam piping in advanced boilers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-509. Producer or source: Vallourec & Mannesmann Tubes Corporation.