Abstract

Lescalloy Hy-Tuf Vac-Arc is vacuum arc remelted. This high-strength steel is used for landing gear, flap tracks, and structural applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-499. Producer or source: Latrobe Steel Company.