Abstract

PX5 is a prehardened steel for plastic molds with superior characteristics in weldability. The steel can be welded in the process of manufacturing a plastics mold without requiring preheating and postheating. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on machining and joining. Filing Code: SA-492. Producer or source: International Mold Steels Inc.