SANDVIK 310/T22 is a composite tube consisting of Type 310 stainless steel for corrosion resistance on the outside diameter and having T22 (21/4 Cr-1Mo) to A213 on the inside diameter to act as the superheater tube and design load carrier. This datasheet provides information on composition. It also includes information on forming and joining. Filing Code: SA-477. Producer or source: Sandvik.