Abstract

YS-T 50 to YS-T 140 Steels comprise a series of high-strength, cold-rolled steels designed to meet performance and weight-saving objectives. They are an extension of Youngstown's series of hot-rolled high-strength steels (see Youngstown YS-T Steel, Alloy Digest SA-261, March 1971). The YS-T 50 to YS-T 140 steels have minimum yield strengths ranging from 50,000 psi to 140,000 psi. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on heat treating, machining, and joining. Filing Code: SA-331. Producer or source: Youngstown Sheet and Tube Company.