Abstract

AISI 8615 is a low-carbon, nickel-chromium-molybdenum alloy steel capable of producing high core strength and toughness. It is a case hardening steel recommended for heavy duty gears, cams, shafts, chains, fasteners, piston pins, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-180. Producer or source: Alloy steel mills and foundries.