Abstract

AISI 9260 is an oil-hardening type of spring steel and tool steel recommended for repeated and severe impact service. It is also used for heavy duty, shock resistant machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-167. Producer or source: Alloy steel mills and foundries.