Abstract

Carpenter No. 709 is a mild chromium-molybdenum, vanadium alloy steel for high temperature service up to 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-125. Producer or source: Carpenter.