Abstract

AISI 3250 is a medium carbon, nickel, chromium alloy steel having high tensile and fatigue strength in the heat treated condition. It is recommended for heavy duty service. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-101. Producer or source: Alloy steel mills and foundries.