Abstract

AISI 5150 is a low-chromium alloy steel, having deep hardenability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-91. Producer or source: Alloy steel mills and foundries.