USS AIRSTEEL X-200 is a very high strength, workable, air hardening steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-85. Producer or source: United States Steel Corporation.