Abstract
LUKENS NINE NICKEL is a 9% nickel steel recommended for low temperature service. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-83. Producer or source: Lukens Steel Company.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International