Abstract

AISI 4320 is a nickel-chromium-molybdenum case hardening steel having high toughness and shock resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-80. Producer or source: Alloy steel mills and foundries.