AISI 9261 is a silicon-manganese shock resisting steel recommended for repeated and severe impact service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-70. Producer or source: Alloy steel mills and foundries.