Abstract

SILMO is a silicon-molybdenum, low carbon steel recommended for applications in which a good combination of high temperature strength and oxidation resistance is required. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-38. Producer or source: Timken Roller Bearing Company.