Abstract

JALTEN is a high-strength low-alloy steel that is readily welded and easily fabricated. It offers an opportunity to incorporate many weight-saving features in design of new products. It is produced in three grades, namely, JALTEN, #1, JALTEN #2, JALTEN #3. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SA-12. Producer or source: Jones & Laughlin Steel Corporation.