TACTIX 740 resin offers high durability for hot melt adhesives. TACTIX 741, an acetone solution of TACTIX 740, is designed for composites prepared by solution prepregging. This datasheet provides information on composition and physical properties. Filing Code: P-32. Producer or source: The Dow Chemical Company, Dow Plastics.