Abstract

MAGNUM 213, MAGNUM 341, MAGNUM 343 and MAGNUM 545 are low-gloss members of the MAGNUM family of ABS resins. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. Filing Code: P-17. Producer or source: The Dow Chemical Company, Dow Plastics.