Abstract

DERAKANE 470-36 and 470-45 resins combine corrosion resistance with superior retention of properties at high temperatures and oxidation resistance. They cure rapidly to give fast green strength and superior creep resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance. Filing Code: P-12. Producer or source: The Dow Chemical Company, Dow Plastics.