GRILON ELX23NZ is a thermoplastic polyamide elastomer with both rigid and elastomeric components. This datasheet provides information on physical properties, and tensile properties as well as fracture toughness. Filing Code: P-11. Producer or source: EMS-American Grilon Inc..