Abstract

GRIVORY G 355 NZ is an unreinforced, amorphous, high-impact resistant engineering thermoplastic. It is opaque and has a natural ivory color. It can be processed by injection molding, extrusion and blow molding. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on casting. Filing Code: P-4. Producer or source: EMS-American Grilon Inc..