Manaurite 50W is a Ni-Fe-Cr alloy for elevated temperatures service. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on wear resistance as well as joining. Filing Code: Ni-745. Producer or source: Manoir Pîtres.