Abstract

DMV 600/600H are nickel alloys with 15.5 Cr. These stable, fully austenitic solid-solution alloys have higher carbon than alloy 600L (See Alloy Digest Ni-702, October 2012). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-721. Producer or source: Salzgitter Mannesmann Stainless Tubes USA Inc..