Abstract

HPM 270 Nickel is a high purity nickel free from nonmetallic inclusions. Its good ductility easily permits significant cold reduction without annealing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ni-686. Producer or source: Hamilton Precision Metals.